Moitzi,
To solve the blister problem first I would need the specifics on the
situation. 1. Board Layup and material type
2. Press ( Vacuum or Conventional)
3. Rate of Rise
4. Type of seperators used
5. Where are the blister occuring in the panel?
between which layer and which sheet of prepreg?
John Haman Jr.
----------
> From: Moitzi Ewald <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] Plisters in Multilayer
> Date: Monday, March 30, 1998 4:08 AM
>
> Hi Technet
>
> Who has experiences in solving plister problems in the laminat of
Multilayers especially for
> single ply construction and thin Multilayer laminats (<0,035").
>
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|