Hi,
What about the solderability of Palladium finished leads on TI devices. I'm
surprised this subject hasn't been discussed on this list! TI are determined
to continue with their lead free technology in spite of the fact that it
doesn't work. Palladium just isn't a highly solderable finish. In spite of
numerous companies finding problems with these devices, it fails to get
discussed! There is a white paper on a TI web site which proclaims the
virtues of this finish. It would make a very interesting basis for a thread
of discussion. http://www.ti.com/sc/docs/asl/palladm