Dear Technetters,
I need all possible help to understand SEM analysis done on my board and to
find out possible sources of basic elements.
(1) On solder mask area, there was Silicon (Si), Sulfur (S) - is it due to
LPI solder mask? Also found Oxygen (O) and Carbon (C)- meaning flux residue?
(2) Found Silicon (Si), Chlorine (Cl), Calcium (Ca), Barium (Ba), Oxygen (O)
and Carbon (C) on epoxy and in a kind of void area- is it from flux?
Is there any book that help me solve above mystery?
re,
ken patel
______________________________________________________
Ken Patel Phone: (408) 490-6804
1708 McCarthy Blvd. Fax: (408) 490-6859
Milpitas, CA 95035 Beeper: (888) 769-1808
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|