To The Engineer Asking About Wave SPC/Metrics:
We at ITT A/CD use the Wave Solder Optimizer. It is a reliable tool
used to monitor/collect important wave solder machine information . .
. i.e. . wave-to-board parallelism, dwell time, immersion depth,
contact length, conveyor speed, preheat temperature, and other
measurements. We ugraded to the Optimizer from the Wave Solder
Analyzer Martin Ingall introduced. Below is the address and a phone
number of a contact for the Wave Solder Optimizer.
Technology Information Corporation
Rebecca Becker
P.O. Box 10121
Silver Spring, MD 20914 USA
TEL: 1-800-768-9283 (SMT-WAVE)
FAX: 301-933-7653
Excellent tool, easy to use.
Ron Hollandsworth
Operations Task Leader
ITT Aerospace/Communication Division
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|