Hi Jens!
FR404 is a FR4 product from AlliedSignal Laminate Systems. They have adopted this material as
their basic (or standard) FR4 product offering for multilayer materials. It is made with woven glass
fabrics e.g. 1080, 2113, 2116, 1652, 7628, etc. impregnated with a multi-functional epoxy resin
system. It is available in all the typical multilayer thicknesses & copper weights, & prepregs. They
don't offer this particular material in standard .059 or .062 rigid laminate any longer. It is also known
as "Gold Lam," since it has an amber or gold color. It has a nominal Tg of 150C. The dielectric
constant varies among the various thicknesses/types from ~4.2 to ~4.9. All the other characteristics
are very similar to other FR4 materials on the market with the same Tg. Call Allied or one of their
reps (e.g. Insulectro) for a data sheet. We have been using it for about 2 years with very good
yields.
Fred J. Paul, Staff Engineer, PCB Operations
FLUKE CORPORATION
P.O. 9090, MS 55, Everett, WA, 98206-9090
direct: 425 356 5734 fax: 425 356 6070 email: [log in to unmask]
>>> VISIT OUR WEB SITE AT WWW.FLUKE.COM <<<
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|