Eltek Ltd. - Process Engineering wrote:-
>Hi !
>We are considering cleaning of innerlayers by adhesive rollers just before
>lay-up . We are applying reduced black oxide , 0.4 mg/sqcm . AOI is done
>before black oxide .
>We allready made preliminary test and we had no problems with delaminations
>etc . My questions are :
>1 ) Does anyone performing similar kind of cleaning after black oxide ?
>2 ) What kind of negative effects should be exepcted ?
>Best regards
>Edward Szpruch
Hi Edward,
We use a tacky roll cleaner prior to lay-up but don't apply adhesive
rollers directly to the reduced oxide layer. IMHO there is the
possibility of adhesive transfer to the oxide surface so a tacky roll
cleaner is better.
Best regards
Paul Gould
Teknacron Circuits Ltd
[log in to unmask]
Isle of Wight,UK
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################