Years ago,
I once had a lot of panels where there were resin voids bridged traces
under the soldermask. These filled up with foam flux (or water from the
wash) and never completely dried. Since the panel had 30 Mohm circuits, we
had intermittant shorts caused by flux and water inside the PCB. This is
the only "flux short" that I have seen.
Aric
-------------
Original Text
From: C=US/A=INTERNET/DDA=ID/ERiemer(a)eskimo.com, on 3/11/98 3:23 PM:
Christy,
For what its worth ...
I've seen intermittent internal shorts in printed wiring boards that were
later found to be
caused by etch defects that had left copper in a ground plane clearance
zone around a via. The
copper was nearly touching the via land but not quite, and when the board
warmed up there was
enough movement to cause the board to short.
Ed Hare
SEM Lab, Inc.
--
SEM Lab, Inc.
Scanning Electron Microscopy and Failure Analysis
Snohomish, WA
(425)335-4400
http://www.eskimo.com/~eriemer/SEMLab.htm
Christy Graham wrote:
> TechNet,
>
> I was told recently of a printed circuit card assembly that, when the
> assembly is powered up in the morning, the board runs, but that by the
> afternoon, it fails. Next day, same board, same results. The engineer
> thinks this problem is due to a "flux short". Is this possible?
>
> Christy Graham
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|