Hi Kathy - I just recieved the following reference (thanks to whoever
mentioned it in a TechNet response!) which you may find helpful:
"Survey of Contact Fretting in Electrical Connnectors", M. Antler, IEEE
Transactions on Components, Hybrids, and Manufacturing Technology, Vol.
CHMT-8, No. 1, March 1985
It doesn't address flash gold specifically but contains a great deal of
info on issues you are facing. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
[log in to unmask] on 03/10/98 06:23:22 PM
Please respond to [log in to unmask]; Please respond to
[log in to unmask]
To: [log in to unmask]
cc: (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
Subject: [TN] Gold Flash vs Gold Plate on PCB connector Fingers
Hey everyone. Can anyone help me out here? Our board vendor is trying
to convince our purchasing department to use gold flash (about 7u"
thick) on the PCB connector fingers instead of gold plate (about 30u"
thick). We make memory boards. These boards will most likely be
plugged in to a system one time, however there could be instances where
they are installed and removed many times. We guarantee our boards for
life. Won't the gold flake off, exposing the nickel and eventually
cause opens if the nickel surface starts to oxidize? Could anyone tell
me where I can find documented proof which supports this theory?
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|