TECHNET Archives

March 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="iso-8859-1"
X-To:
Date:
Wed, 11 Mar 1998 10:22:19 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Eltek Ltd. - Process Engineering" <[log in to unmask]>
Subject:
From:
"Eltek Ltd. - Process Engineering" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (35 lines)
At 17:22 10/03/98 EST, you wrote:
>Hi
>
>Has anyone any information on barrel cracking associated with the use of
> electroless  nickel (EN) under a gold finish. We have a problem with 0.3 mm
> via's in FR4 multilayer boards cracking after thermal shock at 260°C. We have
> other problems with this board but is there any information on what effect EN
> has under these conditions ?
>
>Any comments ?

Chris !
What is the thickness of the copper and what kind of the copper are You
plating ?
Do You perform any heat treatment on the boards before EN ? What about Your
procedures regarding heating of the samples before thermal shock ?
Best regards
Edward Szpruch
Eltek Ltd - Israel
Tel  972 3 9395050
Fax 972 3 9309581
E-mail :  [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2