Jim,
This is one of those "Good News, Bad News" responses.
The "Good News" is that I have found that Chemtronics "Flux Off CZ" is
excellent at removing Rosin Flux residue. The smell is mild but the neat
thing is that it evaporates at a near instantaneous rate. This material
would even work in a vapor degreaser. Kinda reminds me of the old "Freon TE"
days of yore.
The "Bad News" is the cost and product support. I have paid over $400 per
gallon for this material. I think the 55 gal price is around $17K ! The
product support is awful. The guys that make the stuff can't tell you how to
reclaim the material, clean it, or even how to use it. I have one gallon of
"dirty" material that I would like to re-use at some point. If you decide to
use this material, you'll have to set up your own guidelines.
Bill Kasprzak
[log in to unmask]
716-652-2000 ext 2507
716-687-4378 (fax)
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|