At 18:11 11/02/98 EST, you wrote:
>Why do you have a black and a brown oxide process line?
>Using Reduced Black oxide you will be able to process Polyimide type material.
>
>RGregory
>Atotech
>
Gregory !
We do have both black and brown oxide in two diffent tanks . The line is
automatic . As You guessed , we have polyimides and epoxies . The line is
working successfully for 4 years .
Still , what is Your advice regarding rinse water control ?
Best regards
Edward
Edward Szpruch
Eltek Ltd - Israel
Tel 972 3 9395050
Fax 972 3 9309581
E-mail : [log in to unmask]
################################################################