If you run a lot of connectors, you might contaminate your solder pot. The
possible contamination is not just a myth. If you end up whit more than
0.2% of gold in you solder pot, you will have to change it. To much gold
will cause the solder to be grainy and brittle.
At 07:32 10/02/98 -0500, you wrote:
>-- [ From: Tony Bugeja * EMC.Ver #2.5.02 ] --
>
>Is it a big problem running gold connectors in your wave solder? Will it
>contaminate your pot? Or is this just a myth?
>
>Doesn't alot of the gold just end up being dross?
>--
>Tony Bugeja, P.Eng. E-Mail: [log in to unmask]
>Process Engineer Phone: (204) 631-7241
>C-Mac Electronics Fax: (204) 631-7294
>1455 Mountain Ave
>Wpg., Mb. R2X 2Y9
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>
>
------------------------------------------------
Stéphane Richard
Ingénieur de procédés
Process Engineer
Matrox Electronic Systems Ltd
E-mail: [log in to unmask]
Téléphone:(514)969-6000 ext.7585
Pagette : (514)201-0044
Fax: (514)685-3415
-------------------------------------------------
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|