-- [ From: Tony Bugeja * EMC.Ver #2.5.02 ] --
Does anyone have information on soldering silver terminals. We currently use
RMA 615-25 flux an we are getting tarnishing/oxidation when hand or wave
soldered. I looks like the silver is being vaporized off and the brass
below is showing through, the plating thickness is .0003". Is this a
process problem or is it a vendor problem?
--