I have seen the same poor results in the past on paste height measuring
equipment. I would like to throw out a question again --
Has anyone performed a gage R&R (reproducibility and repeatability) study on
this type of equipment with acceptable results?
----------
From: Krishna Kalyan
To: TechNet
Subject: Re: [TN] Assy: Solder Paste Height Measurement
Date: Wednesday, February 11, 1998 4:33PM
Hi everyone.
My two cents worth on LSM. In a project, I found its repeatability
was poor.
krishna kalyan
=====================================================================
>Date: Tue, 10 Feb 1998 18:36:13 -0800
>Reply-To: "TechNet E-Mail Forum." <[log in to unmask]>,
> Ron Lohrbach <[log in to unmask]>
>From: Ron Lohrbach <[log in to unmask]>
>Subject: Re: [TN] Assy: Solder Paste Height Measurement
>To: [log in to unmask]
>
>From: Mark Norris <[log in to unmask]>
>Subject: Re: Measurement Query I thought of interest - Just FYI
>Mime-Version: 1.0
>
>
>A company called cyberoptic makes a real simple height mesuring device,
its
>called LSM (Laser Section Microscope). Used it probably costs 5,000.
>
>
>-------
>At 11:06 AM -0600 2/10/98, Charles Barker wrote:
>>Charles Barker@I-O INC
>>02/10/98 11:06 AM
>>
>>Some years ago, there was a mechanical system on the market for
measuring
>>the height of paste deposited on a pad. The system consisted of a
small
>>granite block, a needle attached to a Mititoyo measuring device that
was
>>moved by a thumbscrew and a monocular 'scope set at about a 30 degree
angle
>>with a back light.
>>
>>The measurement was taken by moving the needle down until it contacted
the
>>top of the paste, zeroing out the Mititoyo, then driving the needle
down
>>until it touched the pad itself. The Mititoyo then read out the
thickness
>>of the paste.
>>
>>Does anyone know of such a simple system out there anymore?
>>
>>TIA
>>
>>Charlie B.
>>
>>################################################################
>>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
>>################################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>>To subscribe: SUBSCRIBE TechNet <your full name>
>>To unsubscribe: SIGNOFF TechNet
>>################################################################
>>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
>>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>>################################################################
>
>
>Ron Lohrbach
>Norris Communications
>(619)679-3137 Tel/VM
>(619)486-3922 FAX
>[log in to unmask]
>http://www.norriscomm.com
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>
______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|