We currently use solder paste when we do rework on PBGA's.
I’m interested in knowing if it is required. I heard that the paste was
not required for PBGA's, only for CBGA's. Is that true ? If so, do we
only have to put flux on the board to be rework before putting the new PBGA ?
Thank in advance.
------------------------------------------------