Dear colleagues:
Sorry, but I have to return to the solder balls spec. issue.
I know, that IPC-S-815B ( 3.6.6) had the criteria for the solder balls (
less than 0.005", no more than 5 per one sq. inch).
Now, IPC-S-815 was replaced by J-STD-001. But , I can not find any solder
balls spec in J -STD.
We are NoClean chemistry users, and will always have tiny solder balls,
although we are trying to reduce its number.
I need an official document to accept presence of the solder balls up to
the certain level, of course.
Please, help!!
Stella Neyman
Eaton Co.
248-608-7289
E-mail: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|