In a message dated 98-02-04 13:38:43 EST, you write:
>
> 4- Can reliability of BGA's (or any other plastic parts for that matter)
> be compromised by exposure to cleaning solvents or solutions?
Sure. Some solvents directly attack plastic. You get changes in the material
properties of the plastic (swell, absorption of solvent, different dielectric
constant, excess leakage). Some cleaning solvents contain varying surfactant
agents to help get under low standoff devices, which in turn must be removed
completely. In some cases, water surface tension prevents water from getting
into the same nooks and crannies that the surfactant gets into. The
surfactants are generally electrically conductive (i.e. leakage) in nature.
Doug Pauls
CSL
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|