TECHNET Archives

February 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Ed Cosper <[log in to unmask]>
Date:
Wed, 4 Feb 1998 12:08:44 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Lenny Kurup <[log in to unmask]>
Subject:
From:
Lenny Kurup <[log in to unmask]>
In-Reply-To:
<01BD3158.ABC2DF00@gateway>
Content-Type:
TEXT/PLAIN; charset=US-ASCII
MIME-Version:
1.0
Parts/Attachments:
TEXT/PLAIN (56 lines)
Hi Ed,

The amp-hour consumption rate, of gold, and any other electroplating
process, depends on the current efficiency of the particular bath. i.e. the
amount of current (amp-hours) actually used for metal deposition, as a
percentage of the current supplied by the rectifier. This efficiency or
inefficiency, must be factored into the calculation for overall
consumption. Getting back to your question, gold plating processes vary
from supplier to supplier and there are different bath types, such as hard
gold and soft or pure gold, the efficiencies vary widely, as well, there
are high speed baths for automatic lines that also vary in efficiencies.

To verify the amp-hour consumption calculations, perform a cathode
effficiency analysis on the bath and base your calculations on the
determined percentage. Additionally, even though your gold supplier states
a particular efficiency, the actual value may be off by as much as 5 % or
sometimes even greater, depending on your operating conditions, and it will
decrease with age.

Regards,
Lenny Kurup
EMX Enterprises Ltd
Markham, Ontario, Canada.
905-475-8000

On Wed, 4 Feb 1998, Ed Cosper wrote:

> Can anyone provide me with information on how many oz of gold per amp hour I should be seeing. I use gold usage vs amp hours as a guide for gold consumption.  I'm basically looking to find  out what  other shops are seeing.
>
> Ed Cosper
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2