Wolfgang;
take a look at the (rough) sketch I have attached - is this the problem you
are describing? If so, the only thing I have ever done to eliminate or
reduce this is to add a microetch step following the acid cleaner in the
electrolytic copper preclean process.
If you don't have a tank available, you can always add .25%-.5% v/v of
hydrogen peroxide to the sulfuric dip; you are not dragging in enough
peroxide to harm the copper bath but you will clean the copper surface
much better. You just need to watch the dwell time...
Hope it helps;
Fred J.
>>> "Erat, Wolfgang" <[log in to unmask]> 02/27/98
01:36pm >>>
We have a customer which is very sensitive to separation between
plated
copper and outerlayer foil copper (doublesided product). This condition
is especially visible at high pad rotation after thermal shock. What can
be done to minimize / avoid this issue ?
Wolfgang Erat / Viasystems Canada
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|