This is the tin in the solder joints complaining (just as you would if you
were dragged into a very hot place then dragged out again, ands then twisted.
At 11:41 26/02/98 PST, you wrote:
>I would like to request for input / feedback on an interesting problem
>that we are seeing sporadically in our SMT line.
>
>Some of the PCBs, post component attach, when they are either in or
>are coming out of the reflow oven are making a "crackling" noise ! We
>have not identified any defects in the boards or the components yet
>and we are unsure what is causing the noise. Sometimes, we are also
>hearing this noise when we take a board in our hands post SMT and try
>to warp it a little ! The boards are approx 5" x 12", have components
>on both sides (passives and some actives) and is not very densely
>populated. Any suggestions on what could be the reason would be
>greatly appreciated !
>
>Thanks,-Koushik Banerjee-
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>
Nicholas Kane
Axion Australasia
Suite 3, 651 Canterbury Road
Surrey Hills
Victoria 3127 Australia
tel: 613 9899 3511 fax: 613 9899 3811
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|