Take a look at:
Antler, M. "Survey of Contact Fretting in Electrical Connectors". IEEE
Transactions on Components, Hybrids March 1985;CHMT-8:87-104.
Mort Antler has done considerable work on fretting of different
metals.
______________________________ Reply Separator _________________________________
Subject: [TN] Mating Tin / Gold; SIMMs and sockets
Author: Non-HP-lee ([log in to unmask]) at HP-ColSprings,mimegw4
Date: 2/24/98 3:01 AM
Ok,
Who has some technical details, study, or white paper on the validity
of, or problems with mating tinned fingered SIMMs with gold contact
sockets or visa-versa? Does this really have any effect on
reliability?
Lee McCuistion
Manufacturing Engineer
Cubix Corporation
2800 Lockheed Way
Carson City, NV 89706
702-888-1000 x237 (voice)
702-888-1002 (fax)
[log in to unmask] (e-mail)
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional inform
ation.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-97
00 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|