BOB HAYNES <[log in to unmask]>
Date:
Tue, 24 Feb 1998 11:43:45 -0600
Content-transfer-encoding:
7BIT
Content-type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, BOB HAYNES <[log in to unmask]>
Parts/Attachments:
text/plain (33 lines)
Ladies and Gentlemen,

This issue was the subject of a lively amount of discussion a couple
of years ago. The question has once again come up in the company I
work for so thought would get the opinion of others. There does not
seem to be any exact guidance in any of the IPC publications that I
am aware of.

When we worked to MIL-C-28809B Par. 3.5.7 left no doubt of what
to do. One was required to bake at 105 Deg. C for an unspecified
time to remove absorbed moisture. Also if the time interval between
baking and soldering was greater than 8 hours you were required to
rebake.

My company set this unspecified time as  12 hours (overnight) and has
continued to use the same process even though most of our production
is now commercial. Also most of the assembly is now surface mount and
when MIL-C-28809 was written (1988) most assembly was TH.

What are other assembly houses doing baking or not baking?

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2