I will try to print glue in perpendicular stripes for SIR testing,
the idea of hand-dispensing many little dots of glue between
SIR traces with a syringe is daunting. I'll let you know how it
works.
----------
> From: ss yeo <[log in to unmask]>
> To: [log in to unmask]
> Subject: Re: [TN] Glue dispenser machine v/s stencil printing
> Date: Friday, March 20, 1998 6:43 AM
>
> Ken Patel wrote:
> >
> > Can anyone tell me what Motorola is using to dispense the glue
(epoxy)on
> > solder side, glue dispenser or trough stencil printing? Does anyone
know any
> > contact house uses glue printing method?
> >
> > Any help will be appreciated.
> >
> > re,
> > ken patel
> > ______________________________________________________
> > Ken Patel Phone: (408) 490-6804
> > 1708 McCarthy Blvd. Fax: (408) 490-6859
> > Milpitas, CA 95035 Beeper: (888) 769-1808
> >
> > ################################################################
> > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> > ################################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> > To subscribe: SUBSCRIBE TechNet <your full name>
> > To unsubscribe: SIGNOFF TechNet
> > ################################################################
> > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
> > For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> > ################################################################
> Hi Ken,
> I am using screen printing for epoxy in my facility. It works
just as
> well and to a certain extent it is faster. Only draw back i see is the
> wastage in epoxy.
> Do not know what Motorola is so I can't help you there
>
> ss
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|