Now we used tenting plating process for made circuit board.
In this process used for univesal MS ADDITIVE at atotech com.
Now current density 2.7A/dm2, Total ampere 1200AMP.
But when now plating, happend roughness plating, as liek residual Cu at
surface ,
It' looks like particle of Copper by burning at plating bath.
It makes a open at imaging process,
I guess it relations with air agitation, leveller, carrier concentration
of copper plating bath.
But analasys datum have no N.G .
what can I do efficience easily removes that.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|