Matt: I have seen this same or similar condition on gold features. We
use a different LPI than you, applied by a DP10. Ni and Au are electrodeposited;
150u" and 30u" respectively. This happens only on a certain style of consruction
and in our case had nothing to do with developing, although we went up and down
that road quite a few times. If you would like to discuss this further contact
me.
Regards
Michael Barmuta
Staff Engineer
Fluke Electronics
Everett Wa.
425-356-6076
On Thu, 12 Feb 1998 13:42:10 -0800 Matthew Byrne wrote:
> From: Matthew Byrne <[log in to unmask]>
> Date: Thu, 12 Feb 1998 13:42:10 -0800
> Subject: [TN] Re[4]: [TN] Soldermask developing
> To: [log in to unmask]
>
> I am using Taiyo AUS-5 on electrolytic nickel gold. Yes, we would
> like to do selective plating, but the parts cannot be bussed. We are
> required on this part to use electrolytic full-body gold & the Taiyo
> mask.
>
> Electrolytic gold is not very smooth when examined microscopically.
> There seems to be many cracks & crevices to get into & trap material.
>
>
> Matt Byrne
> HADCO
> ______________________________ Reply Separator
_________________________________
> Subject: Re: [TN] Re[2]: [TN] Soldermask developing
> Author: "TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask] at
> SMTPLINK-HADCO
> Date: 2/11/98 11:33 PM
>
>
> You did not specify whether your gold was electrolytic (usually a thicker
> deposit and less porous) or the electroless Ni/Au (usually thinner [up to 5
> microinches] and more porous). I would expect that there would be no problems
> with developing mask off the electrolytic gold and there could be more
> problems with the more porous electroless Ni/Au.
>
> Most people who use gold circuitry will selectively gold plate (electrolytic)
> or will plate the electroless Ni/Au after the solder mask has been applied and
> cured. Let's face it, gold is expensive and the less you can get away with and
> still satisfy the customer, the better for the bottom line.
>
> I have not heard of developing LPI mask off of gold (not a whole lot of
> experience here, either). Perhaps, you may need to develop more aggressively
> or look at other LPI solder masks.
>
> Larry Fisher
> Dexter Electronic Materials
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
text
> in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
> information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|