I have an Alpha Metals Ionograph model 500M that I have inherited from
an engineer that is no longer with the company. Along with this piece
of equipment I have only inherited internal procedures that look like
they have been copied from the manual, but no manual.
We have to calibrate or verify the solution by taking a specific gravity
and running the test procedure. in this you use the reading you have
taken above and add a know amount of contaminate to the unit. I am then
looking for a reading of 37.5 (+/- something I'm assuming) for a pass.
the problem I am having is that I am reading in the 420's to 460's and
no one here has ever seen this unit fail. we also do not cover the fail
contingency in our procedures. I have been leaving messages with Alpha
Metals for 2 days with no reply.
Help!!!!!!!!!!!!!!!!!!!! Has anyone encountered this and if so could you
give me some guidance.
Bill Irwin
[log in to unmask]
Bill Irwin
Berg Electronics
(717) 764-7309
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|