Edward, I agree with Mr. Gregory of Atotech that there should be no
reason that you cannot process FR-4 materials and polyimide with the
same reduced brown oxide. The only material that I have been unable to
use with reduced oxide is cyanate ester.
I have had very poor success using conductivity control for these types
of rinses. I also strongly recommend against using DI water for rinsing
following DMAB - I have seen problems with yellowish staining of the
reduced oxide when using DI. I have had my best success using a pH
controlled rinse of between 3 and 4 pH units following the oxide; this
scavenges the chlorite from the oxide deposit as well as removing the
hydroxide from the surface. This chlorite will destabilize the very
expensive DMAB; using a pH controlled rinse can reduce consumption of
the DMAB by a very large amount. Following the DMAB I have sometimes
used a pH controller to maintain the rinse tank below 7 pH, and once
again have ALWAYS used soft or tap water for this rinsing.
Good luck
Fred J.
In case you didn't catch it the first two times, I NEVER USE DI WATER
FOR RINSING AFTER THE DMAB!!!!
>>> "Eltek Ltd. - Process Engineering"
<[log in to unmask]> 02/11/98 10:40am >>>
Hi Technetters !
Our black/brown oxide line is operating with baskets . The final sequence
of
black oxide process include :
black oxide , cascade rinse with DI water , DMAB reducer , cascade
rinse
with DI water , static DI hot water , dryer .
The final sequence of brown oxide process include :
brown oxide , cascade rinse with DI water , , static DI hot water , dryer .
We are planning to regulate DI water replenishment in flowing rinses and
static hot water rinse by conductivity control .
What values of conductivity should be considered ?
All comments will be appreciated
Regards
Edward Szpruch
Eltek Ltd - Israel
Tel 972 3 9395050
Fax 972 3 9309581
E-mail : [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|