TECHNET Archives

February 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Bernard Kessler & Associates LTD <[log in to unmask]>
Date:
Wed, 11 Feb 1998 10:36:26 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bernard Kessler & Associates LTD <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Hi----
Re Dan LeVasseur's question----

"GEB" is the designation for the old NEMA G11 laminate ---- the very original GE
hetanhydride resin system laminate which served as the very first flame
retardant laminates.  Devil on drills and routing blades.  If I recall correctly
---- or at all ---- the big difference between the G10 and the G11 was the flex
strength retention but this is my best guess.    The G11 was essentially
replaced by the "GF" or NEMA FR4 because most of the usage was related to the
flame retardancy ----- not necessarily its mechanical strength.

Enjoy!!

Bernie Kessler

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2