Richard,
We have a lamination press made by Burkle (model: LAMEV 100). It is a 4 opening press with a closed vacuum chamber.
In general I am pleased with it - in is reliable (except for corrosion problems in the cooling system), has good MMI (through a PC) and easy to operate.
The press gives good results as to temperature uniformity over the hot plates and has special features to use when producing boards smaller then the press platen intself.
The only (rather severe) problem we had encountered is corrosion in the cooling water piping - it hits you usually unprepared and, because the press has a closed vacuum chamber, you have to take it apart (almost) in order to get to the cooling system.
Please contact me directly or through this forum with specific questions and I will be happy to assist you.
Best regards,
Yehuda Weisz
-----Original Message-----
From: Richard MacCutcheon [SMTP:[log in to unmask]]
Sent: 9 פברואר, 1998 20:24
To: [log in to unmask]
Subject: [TN] Lamination Presses Input
We are beginning the process of
replacing our 20 year old lamination
press with a new Vacuum press.
I need input, good or bad, about the
various suppliers of such equipment and
any experiences you may have
All info will be regarded as valuable.
Thanks for your time and information.
Richard MacCutcheon
BFGoodrich Aerospace
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
*************************************
* Yehuda E. Weisz
* e-mail: [log in to unmask]
* Tel: 972-3-6342045
************************************
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|