TECHNET Archives

February 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Fri, 6 Feb 1998 21:42:55 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
"Phillip E. Hinton" <[log in to unmask]>
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (27 lines)
Carlos,

The idea of many users today is that an edge boad connector is not inserted
more than twice.  Once for functional test and once for insertion in the
equipment.
If any problem occurs after that, take it out and discard it.  Sometime the
functional test is skipped.  For this application the 5 microinches of gold is
sufficient provided the environment of use is not very harsh.  If you want
many insertions you better go with the thicker gold.  The old rule of thumb
was: The total number of insertions plus the number of extractions required
should be equal to the gold thickness in microinches.  So if you wanted fifty
insertions you would put on 100 microinches of gold use.

Phil Hinton

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2