TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
TechNet Mail Forum.
Date:
Wed, 7 Jan 1998 23:07:42 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (82 lines)
>Hi Jens - We need some additional information to help provide you possible
>solutions:
>
>1) What type of gold and thickness?

Immersion (chemical) gold. Very thin I presume.

>2) Is there an underplate (type & thickness)?

Ni

>3) What is the soldering process specifics the board is subjected too (flux
>type, conveyor speed, etc)?

Well, the had the same PCB in HAL. I'm sure they did not do any adjustments
to the solder machine.

>4) What are the board specifics (thickness, type, # of inner layers, hole
>dimenstions, etc.)?

Very simple 4 ML PCB, 1.60mm. In my opinion a D/S board would be OK.


Jens Behrens



>
>
>Hi All,
>I got a problem with solderability!
>We where selling a HAL PCB for a few years. Since it was gold contacts too,
>we suggested to the customer to change to gold plating.
>After he got samples he claims that the solderability (wetting) is not very
>good.
>The PCB is wave soldered.
>Any comments are welcome.
>Best regards
>Jens Behrens
>
>
>        ==========================================
>        Jens Behrens    URL HTTP://www.felsweb.com
>        Fels Ltd.       Tel.: +(852) 2423-1812
>        GPO Box 8721    Fax.: +(852) 2423-1899
>        Hong Kong       [log in to unmask]
>        ==========================================
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>##############################################################
>
>
>
>
>
>
>
>
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################