Liquid-liquid is more accelerated. This is because the heat transfer of the
perfluoronated liquid is much better than air. Thus, the rate of change is
faster. This causes higher thermal stresses. The use of accelerated life
tests is to reduce test time & cost (sample size). You can find failures
that may take 100's of parts and 1000's of hrs to find. The only thing you
have to watch out for is failures that would never happen in the field.
----------
> From: Scott Westheimer-CTUA143 <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] Thermal cycling
> Date: Tuesday, January 06, 1998 1:06 AM
>
> Can anyone tell me the difference between thermal cycling in
liquid/liquid
> or air/air. Is there a different failure mode associated with each
process?.
> Meaning, if a sample passing one but fails the other what would be the
> reasons?
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|