In a message dated 98-01-28 11:08:02 EST, you write:
>
> One simple method of protecting stamped inks is mask them
> using peelable-latex soldermask that is used for
> wavesoldering application. Let it dry prior to a cleaning
> cycle and remove the mask afterward.
The only caution I would give here is that many of the peelable-latex masks
leave chloride residues behind. Not a good idea and I don't know how well
these residues would come off in a 200-proof alcohol wash.
Doug Pauls