Low pressure areas can be difficult sometimes, have you tried the specialized
press pads designed to even the pressure distribution across the panels ? There
are many on the market and they do work very well (from experience). I have
been successful using these to press up to 5oz. copper internally with minimal
resin voids.
Tony King