Steve,

Call me offline about this. Sounds like something we can help you with.

Sincerely,

Paul Terranova

DIGITAL's Analytical and Environmental Test Services Lab
Phone: 508-467-3109
FAX: 508-467-6796
[log in to unmask]

> -----Original Message-----
> From: Tucker, Steve (KS) [SMTP:[log in to unmask]]
> Sent: Monday, January 19, 1998 6:50 PM
> To:   [log in to unmask]
> Subject:      PCB Solderability Analysis
>
> Hello Technetters,
>
> I have been experiencing considerable defects across the wave solder
> with one particular vendors PCB's. My question is what guidelines are
> most commonly used to perform a solderability analysis and can anyone
> suggest a good lab for having this done.
>
> Thanks in advance,
>
>                       Steve Tucker
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################

ATOM RSS1 RSS2