Try a UV curable adhesive. We're using a Masterbond product UV15-7TK1A. It is
a one-part epoxy which cures in about 30 seconds when subjected to a UV light.
It is low-flow (it stays where you put it), solvent resistant, and can be
removed after cure, if necessary.
##############################################################