Hi Dave - You have me confused! What is BuCu? I'll take a guess that you
didn't invent a new element and were shooting for BeCu! Brush Wellman and
NGK Berylco both have some very good technical information on the BeCu
(corrosion, mechanical, formability, etc.). Brush Wellman's number is
216-486-4200 and NGK 's number is 215-921-5000. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
[log in to unmask] on 01/19/98 01:19:54 PM
Please respond to [log in to unmask]; Please respond to
[log in to unmask]
To: [log in to unmask]
cc: (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
Subject: [TN] BuCu for flex circuits
Hi Technetters
Does anyone out there have any information on BuCu for flex circuits. I'm
interested in processing issues both for the circuit manufacturer and the
board
fabricator. Also of interest are the properties of this material and the
reasons one would choose it. Any information at all will be greatly
appreciated.
Thanks in advance,
Dave Tyler
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|