TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Thu, 15 Jan 1998 16:30:17 -0700
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, John Maxwell <[log in to unmask]>
Subject:
From:
John Maxwell <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (32 lines)
Reduce the amount of solder stenciled on the pads prior to placement.
Typically a 35% reduction in the stencil opening is enough to fix this type
of peoble. Be sure to keep solder paste under the terminations to insure
paste/flux contact to that metalization prior to reflow.

Regards,


John Maxwell

>     We have been experiencing problems with tombstoning of 1210 caps.  I
>     have not been able to find any information about parts this large
>     tombstoning.  Is there any way to fix this problem while we are
>     waiting for a design change to the pad layout?
>
>     Any help on this subject will be greatly appreciated.
>
>     Sean Gearin
>     [log in to unmask]
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################

ATOM RSS1 RSS2