Alan,
Your question has raised another one I have. We have some products with carbon
ink for button contact. We also use no-clean, but have tended to use water
soluble for these products to eliminate residues on the carbon ink surface. Do
you mask the carbon ink before fluxing or does the no-clean residue pose no
problems for button contact?
Regards Evan
Evan Jones
Manufacturing Engineer
IBM Wangaratta
Ph 61 3 5720 2539 Fax 61 3 5720 2412
Email [log in to unmask]
---------------------- Forwarded by Evan Jones/Australia/IBM on 08/01/98 08:49
---------------------------
[log in to unmask] on 07/01/98 21:59:35
Please respond to [log in to unmask] @ internet
To: [log in to unmask] @ internet
cc:
Subject: [TN] Gold Flash benefits over HAL
We are wave soldering double sided PHT boards using a No Clean flux.
There is a proposal to replace the hot air levelled solder over bare
copper(HAL ) finish with gold flash, about 5u inch thick, over 100u inch
of nickel.
The proposal would allow us to drop the carbon ink screening requirement
used for contacts to a rubber keypad.
I see no other benefits to this, only the following problems:- gold
contamination of the solder pot and weaker solder joint strength. Does
anyone know of any other benefits?
Alan Shaw
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe:
SIGNOFF TECHNET ##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information. For the technical support contact Dmitriy Sklyar at [log in to unmask]
or 847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|