An oxymoron? ...
Does anyone know of a combination persulfate microetch and acid cleaner?
I want to introduce some old equipment and have limited chambers.
By leaving copper in acid cleaners one can introduce an etch, but
smutting occurs in the ones I am familiar with.
Thank you,
J Warhelere
[log in to unmask]
##############################################################