TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Wed, 7 Jan 1998 06:41:11 -0500
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
john balchunas <[log in to unmask]>
X-cc:
Content-Type:
text/plain; charset=us-ascii
Organization:
john balchunas
MIME-Version:
1.0
Parts/Attachments:
text/plain (30 lines)
Hello Krishna,

Is the secondary side in contact with the oven's conveyor rack?  SMDs
and primary side thru-hole leads can bind and slip during transport.
Support the board with a fixture or use the rails if you're not doing so
already.

You can also check the solderability of your pads.  Print some paste at
the problem site on a bare board and look for good wetting after
reflow.  If the solder balls-up, you've found the culprit.  Choose a
sample with grainy-looking pads from the problem lot if possible.  That
is one indicator of exposed, unsolderable intermetallic on a hot air
solder leveled board (HASL).  There should be at least 80 microinches of
Sn63/Pb37 coating the pads for good solderability in a JIT process.
I've used Trace Labs in Chicago for this kind of testing before.

John Balchunas

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2