TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Matthew Park <[log in to unmask]>
Date:
Tue, 6 Jan 1998 15:41:49 -0800
Content-Type:
text/plain
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Matthew Park <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
Joe,

The problem you mentioned using tin/lead board finish is
nothing new ( from what I can remember working for my
previous empolyer a long ago).  Wrinkling of boards is very
problematic in addition with non-wetting surfaces. You may
need to scrub your bare boards prior the assembly.  Get
yourself a bunch of good brushes....
Try soaking tin/lead finish bare boards in alcohol-based or
flux removing solvent.  This will remove grease and foreign
contaminants. You will see solderability improvement for
wavesoldering.
Using a more active flux is another option for that finish.
RMA flux (high solid content) or water-soluble flux will
definitely work good but need freon cleaning or washing.

regards
Matthew Park

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2