TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Matthew Park <[log in to unmask]>
Date:
Wed, 28 Jan 1998 08:04:39 -0800
Content-Type:
text/plain
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Matthew Park <[log in to unmask]>
Parts/Attachments:
text/plain (73 lines)
Bob,

One simple method of protecting stamped inks is mask them
using peelable-latex soldermask that is used for
wavesoldering application.  Let it dry prior to a cleaning
cycle and remove the mask afterward.

regards
Matthew Park
NII Norsat International Inc.

>>> Ferrell-2 Bobby
<[log in to unmask]> January 28, 1998
5:22 am >>>
Hello Technetters,
Any suggestions on the following problem would be greatly
appreicated.

We are manufacturing/assembling small amounts of custom
boards in house
and are having a
problem with the ink stamped serial numbers on the board.
We have tried
several different types of coatings (epoxies, varnishes, etc.)
to try
and protect the ink stampings from coming off.  The
difficulty that we are having now is that during a cleaning bath
in 200
proof alchol the epoxy is
peeling off.

Does anybody out there have any suggestions as to what to
use to protect
the ink stampings.

TIA,


Bob Ferrell
NASA
MM-G1/G3
Kennedy Space Center, FL.  32899
407-867-6678

>

################################################################
TechNet E-Mail Forum provided as a free service by IPC
using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at
[log in to unmask] or 847-509-9700 ext.311
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2