Hi All,
The pads of PBGA`s that we use are defined by solder mask on our
multilayer FR4 pcb`s
The diameter of stensil aperture is bigger than the pad diameter , so we
are actually printing
( no-clean ) paste on the soldermask.
Is this OK, or should it be avoided ? I presume that the adhesion between
stensil
aperture-paste is bigger than the other one between soldermask and paste,
resulting
to increased risk to solder balls, which could be fatal under PBGA ( pitch
.05" )
Stencil width is 0.15 mm ( 6 Mils ), laser cut
Stensil diameter .56 mm ( 0.22" )
Pad diameter 0.72 mm ( 0.28" ) max
Solder Mask diameter 0.52 mm ( 0.20" )
Any opinions?
Brs, Johannes
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|