MOST SMT COMPONENTS ARE PLASTIC PACKAGES .
I HAD EXPERIENCED REMOVAL OF COMPONENT MARKING ONCE THE
COMPONENTS ARE EXPOSED TO ACETONE AT 40-50 DEG C EVEN FOR SHORT
DURATIONS. ACETONE IS CORROSIVE EVEN TO SS.
IT MIGHT AFFECT RELIABILITY(CORROSION) AS PLASTIC PACKAGES MIGHT ABSORB
SOLVENT .
> ----------
> From: Chan, Marcelo[SMTP:[log in to unmask]]
> Sent: January 27, 1998 2:39 PM
> To: [log in to unmask]
> Subject: [TN] Acetone of SMT assemblies
>
> What are the drawbacks to using Acetone as a solvent on a fully
> assembled PWB with surface mount components? The idea is to dip the
> entire assembly for about 15 minutes....Would the epoxy molding on
> components absorb the acetone? What about the soldermask?
>
> Marcelo
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|