Once we've came across this subject the problem was cheap ( step in
process missing ) solder mask = fabrication .
I'd reject it all , especially if you go with it over solder pot , the
cracks do seep the solder underneath , peeling the mask in the process .
Otherwise it corrodes in time , and breaks down further still .
Definitely not the boards you want in medical devices ( class 2?) .
Paul Klasek
ResMed , process eng.
>----------
>From: Arif[SMTP:[log in to unmask]]
>Sent: Tuesday, 27 January 1998 10:29
>To: [log in to unmask]
>Subject: [TN] IPC question
>
>Hi there,
>We are a medial device manufacturer and we're getting our finished PCB
>assemblies via a local vendor.
>We are getting many rejects as we try to implement IPC-A-610. Our trouble is
>in 7.2.3 solder mask coating
>breakdown.
>
>MY QUESTION:
>
>We are getting a small areas of exposed copper. Stuff you can't see with the
>naked eye. This is due to
>either PCB fabrication or assembly process. IS THERE AN ACCEPTABLE EXPOSED
>AREA THAT
>CANNOT BE EXCEEDED OR SHOULD ANY EXPOSED COOPER NO MATTER HOW SMALL
>IT IS BE REJECTED.
>
>Thank you for your time and I look forward to getting an answer soon.
>
>Arif Quronfleh
>Sr. Project engineer
>NeuroCare Group
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|