Dave,
We have had some luck locating high resistance under flip chip using
thermal imaging, but could not use the technique to find hard opens.
We also put some effort into time domain reflectometry to locate opens
with little success, but the technique could possibly work with
further refinement.
Rod Martens
Hewlett-Packard Co.
Fort Collins, CO
______________________________ Reply Separator _________________________________
Subject: [TN] Finding shorts & opens inside PWB's
Author: Non-HP-dkleinman ([log in to unmask]) at HP-ColSprings,mimegw4
Date: 1/22/98 2:54 PM
Hi People,
Does anyone have precise methods of isolating locations of shorts and opens
inside a finished PWB. Electrical Test, Probots and Micro-Ohmmeters hint at the
areas of the defects, but dont reveal the actual location. I am wondering if
anyone has tried Infared Thermal Imaging, High Resolution x-ray or Tracing high
frequency signals through a board. New project and little frustrated, Thanks
for any help.
Dave Kleinman
Optical Inspection Engineer
Raytheon-TI Austin, TX
512-250-7141
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional inf
ormation.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-97
00 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|