TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 16 Jan 1998 11:55:02 EST
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, SABowles <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
SABowles <[log in to unmask]>
Organization:
AOL (http://www.aol.com)
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (27 lines)
Andy,

Arlon's 85NT is a non-MDA polyimide on aramid non-woven reinforcement.  The
properties are as follows:
Tg - approx. 250 C.
Dk - 3.9
CTE for X and Y is around 8-10ppm per degree C.  Z is rated around 100ppm.

Arlon's 55NT is a multifunctional epoxy on aramid non-woven reinforcement

Tg - approx. 180 C.
Dk - 3.9
CTE for X and Y is around 8 -10ppm per degree C.  Z is rated aorund 100ppm.

Scott

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################

ATOM RSS1 RSS2