We sent 2 types of samples to UL Lab for 94V-0 Approval. One type
of samples passed but the other type failed.
The samples which passed the 94V-0 test were 10 pcs of 10-layer FR4
multilayer boards without solder mask or copper circuit. The
total Flaming for applications (Set of 5 specimens) are 15 sec
(23 +/- 2 deg C and 50 +/- 5% RH for 48 hrs) and 12 sec (168 hrs
air oven at 70 +/- 1 deg C then cooled in a dessicator for at
least 4 hrs)
The samples which failed the 94V-0 test were 10 pcs of 10-layer
FR4 multilayer boards coated with solder mask. The total Flaming
for applications (Set of 5 specimens) are 32 sec (23 +/- 2 deg C
and 50 +/- 5% RH for 48 hrs) and 48 sec (168 hrs air oven at 70
+/- 1 deg C then cooled in a dessicator for at least 4 hrs)
The materials we used are :
Laminate: Isola E-Cu#104ML
Prepreg: Isola E#104ML
Solder Mask: Lea Ronal OPSR 5600 GDA
All the materials are UL 94V-0 approved. I think there could be
something wrong on our processing, e.g. solder mask over post bake,
too much thinner, improper thinner, etc. We use the thinner:
Butyl Icinol at 3-5%.
What process settings may affect the 94V-0 test result?
Is there anybody can help ?
Thank you
Chan Chi Man
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|