TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Fri, 9 Jan 1998 06:48:04 -0500
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
john balchunas <[log in to unmask]>
X-cc:
Content-Type:
text/plain; charset=us-ascii
Organization:
john balchunas
MIME-Version:
1.0
Parts/Attachments:
text/plain (38 lines)
Try Glenbrook Technologies in Morris Plains NJ:
http://www.glenbrooktech.thomasregister.com/olc/glenbrooktech/

Send them a few boards to X-ray and use the images to decide if there
are any voids, shorts or insufficient fillets to worry about.  Their
service is next day and very affordable.

You can also consider sampling your SMT output with an in-circuit-test
like GenRad if you have one available.

John Balchunas

> Date:    Thu, 8 Jan 1998 17:13:38 PST
> From:    Krishna Kalyan <[log in to unmask]>
> Subject: Cold Solder and Solder Shorts
>
> Tech Netters :
>    Hello all. Can you tell me a practical way to differentiate between
> between a cold solder and a small skew (but large enough to cause an
> electrical open) on components such as 0603, 0402s ?
>
> Thanks
>
> Regards
> Krishna Kalyan

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2